Nimonic 80A / NiCr20TiAl(2.4952) / UNS N07080/ BS 3HR1

Nimonic 80A / NiCr20TiAl(2.4952) / UNS N07080/ BS 3HR1

Subgroup:

$1.00
Dimensions: OD:50mm x L
Lead Time: About 60 days
GE spec NB 00146, Ideally released to GE spec NB 00146 or to ASTM B637 or WK 2 4952 or BS 3HR1, VIM+ESR, Hot Forging,Polishing,
  • Descriprion
  • Product Details
GE spec NB 00146, Ideally released to GE spec NB 00146 or  to ASTM B637 or WK 2.4952 or BS 3HR1, VIM+ESR, Hot Forging,Polishing,

Grade

2.4952

Nimonic 80A

C

0.04~0.10

0.10

Si

1.00

1.00

Mn

1.00

1.00

P

0.020

S

0.015

0.015

Ni

65.00

Balance

Cr

18.00~21.00

18.00~21.00

Ti

1.80~2.70

1.80~2.70

Al

1.00~1.80

1.00~1.80

Co

1.00

2.00

Fe

1.50

3.00

Cu

0.20

0.20

B

0.008

0.008

Zr

0.15

Pb

0.0025


Quick Details

  • Standard:
  • Melt Practice:
  • ---下拉选择---
  • shape:
  • ---下拉选择---
  • Heat Treatment:
  • ---下拉选择---
  • Surface:

Supply Ability

  • Supply Ability:
  • 300 Ton/Tons per Month Nimonic 80A / NiCr20TiAl(2.4952) / UNS N07080/ BS 3HR1

Send your message to Longhai Special Steel