2570


2570 material is SS SS 142570 High-strength austenitic steel for use at elevated temperature High-strength austenitic steel for use at elevated temperature.

Chemical composition of 2570, 2570 mechanical properties, 2570 datasheet, 2570 equivalent grade, Heat treatment and temperature process of 2570.


2570 property sheet

2570 Spec.

SS SS 142570
High-strength austenitic steel for use at elevated temperature

Chemical Composition of 2570

C: Max 0.08
Si: Max 1.00
Mn: Max 2.00
P: Max 0.025
S: Max 0.025
Cr: 13.50 16.00
Ni: 24.00 27.00
Mo: 1.00 1.50
V: 0.10 0.50
Ti: 1.90 2.30
Al: Max 0.35
B: 0.003 0.010

Mechanical Properties of 2570

Rp0.2 (MPa) 972 (≥)
Rm (MPa) 931 (≥)
AKV (J) 43
A (%) 24
Z (%) 31
Hardness HBW 334

2570 shape and dimensions

2570 Round bar: 1mm-800mm
2570 Square bar: 10mm * 10mm-600mm *600mm
2570 Flat bar: Thickness:8mm-800mm Width:10mm to 1500mm
2570 Sheet or Plate: Thickness:3mm-80mm Width:1.5mm to 1500mm
2570 Strip or Coil: Thickness:0.1mm-3mm Width:1.5mm-1500mm
2570 Forgings: Shafts with flanks/pipes/tubes/slugs/donuts/cubes/other shapes